Metal Film Resistors (Precision) Carbon Film Resistors How To Apply Resistors Zero OHM Resistors Metal Oxide Resistors Metal Film Resistors How To Order Moulded Metal Film Resistors Metal Glaze Resistors Products
 
Metal Oxide Resistors
 
TEST PROCEDURE GENERAL PURPOSE
MO25, MO50, MOS50, MO100,
MOS100, MO200, MOS200
SHALL NOT EXCEED
Operating Temp. Range - 55°C to + 200°C  -
Temp. Coefficient (ppm/C) 100, 200 -
Short Time Overload 2.5 X rated Voltage
Duration - 5 seconds
imageR = ±(1 % + 0.05 Image)
Resistance to Soldering Heat Temp : 260°C ± 5°C
Duration - 10 seconds
imageR = ±(1 % + 0.05 Image)
Temp. Cycling 5 Cycles of -55°C, +25°C, +200°C, +25°C imageR = ±(1 % + 0.05 Image)
Moisture Resistance 40°C, 95% relative humidity,
Duration - 56 days
imageR = ± 3% 
Load Life Rated Voltage at 70°C ambient
Duration - 1000 hrs.
Condition : 1.5 hrs. ON 0.5 hr off
imageR = ± 3%
Dielectric withstanding Voltage V-Block Method, 3 x Limiting Voltage
Duration - 1 minute
imageR = ±(0.5 % + 0.05 Image)
Insulation Resistance V-Block Method, DC 500V
Duration - 1 minute
> 104Image
Non Combustibility The resistor shall withstand Overload test of 10 times Rated Voltage for 5 Sec.
 
Derating Curve

© 1999 MFR Electronic Components Pvt. Ltd.